The production process of flat toothpicks in 1955.
preserve of row material birch wood in pool
cut a timber to 30 cm with hanging saw
3. boiling timber in hot water for 24 hours to make it soft
4. peeling a timber to sheet 1mm thickness by rotary machine
& cut to 50 mm in width
5. punching machine by iron blade to form flat toothpick
6. dry wet toothpick by sunshine
7. after dry, polish them to make smooth in machine
8. arrange the disordered toothpicks in line
9. package in box for export